• Skip to primary navigation
  • Skip to content

00 34 91 842 94 67

(opens in new tab) (opens in new tab)
MENUMENU
  • Español
    • English
    • Français
Logo-sti
  • Análisis de superficie
    • Microscopios de fuerza atómica
      • Nano-Observer
      • Modos eléctricos avanzados para AFM
      • Entornos
      • Puntas AFM
      • AFM IR
    • Perfilometría óptica
      • Perfilometría óptica
      • Medición dinámica
    • Perfilometría mecánica
    • Medición de película delgada
      • Reflectometría (Medida de espesor de capa delgada)
      • Mapeo de resistividad y conductividad
    • Nanoindentadores
    • Sistemas de Vacío
      • Sistemas de deposición
      • Sistemas de análisis
      • Accesorios e instrumentos UHV
    • Espectroscopia IR & RAMAN
      • AFM IR
      • Infrarrojo
      • RAMAN
  • Nuestros servicios
  • Formación
  • Servicio postventa
  • Empresa
    • ScienTec Ibérica
    • Eventos 2020
    • Noticias
  • Contacto

Vous êtes ici : Accueil > Produits > Nanoindentador hasta 50 mN de fuerza

Nanoindentador hasta 50 mN de fuerza

Inano

El nanoindentador perfecto para capa fina y polímeros!

iNano

1. Preciso, flexible y fácil de usar
2. Amplia gama de pruebas nanomecánicas.
3. películas delgadas y materiales blandos

 

El naonindentador INano es un instrumento preciso, flexible y fácil de usar que permite una amplia gama de pruebas nanomecánicas, incluido el módulo y la dureza (Oliver y Pharr, ISO 14577), el módulo de almacenamiento y pérdida y las pruebas universales. El iNano puede ejercer hasta 50 mN de fuerza para probar películas delgadas y materiales blandos. Fácil de usar, el iNano ofrece una solución llave en mano que ofrece precisión y precisión, lo que permite realizar pruebas nanomecánicas superiores en todos los laboratorios, desde las universidades más grandes hasta las empresas de alta tecnología.

 

Nanoindentation

Imicro far

iMicro : Nanoindentación hasta 1 N de fuerza >>

G200 kt

G200 : Nanoindentador para la nanoescala >>

Nanoflip-5

NanoFlip : Nanoindenter ambiental y de vacío >>

Nanoindentation

InSEM HT : Nanoindenter para alta temperatura >>

Icon_Scientec-03

Necesitas ayuda ?

Contáctanos >>

Aplicaciones Caracteristicas Opciones

Aplicaciones de nanoindentación

  • Mediciones de dureza y módulo (Oliver-Pharr)
  • Tarjetas de propiedad de hardware de alta velocidad
  • Prueba de dureza ISO 14577
  • Polímero Delta, módulo de almacenamiento y pérdida
  • Pruebas cuantitativas de arañazos y desgaste
  • Prueba de nanoindentación a alta temperatura
  • Industrias

    • Recubrimientos duros
    • Obleas de semiconductores
    • Cerámica y Vasos
    • metales y aleaciones
    • Baterías y almacenamiento de energía.
    • Investigación y desarrollo
    • Farmacia, alimentación y cuidado personal.
    • Automotriz y aeroespacial
    • Ensayos universales a nanoescala
Imicro - applications - hardness and modulus measurements

Imicro - applications - hardness and modulus measurements

2 property maps

2 property maps

Imicro - applications - iso 14577 hardness testing

Imicro - applications - iso 14577 hardness testing

3 complex shear modulus of compliant biomaterials

3 complex shear modulus of compliant biomaterials

Scratch pack 2

Scratch pack 2

Inano - options - sample heating

Inano - options - sample heating

Mems

Mems

Más información sobre aplicaciones

- Adhesión

- Dureza

- Young module

- Rasguño

Nanoindentación con fuerza hasta 50 mN

Nanoindentación con fuerza hasta 50 mN
El iNano® Nanoindenter facilita la medición de películas delgadas, recubrimientos y pequeños volúmenes de material. El instrumento preciso, flexible y fácil de usar puede realizar una amplia gama de pruebas mecánicas a nanoescala, que incluyen muescas, durezas, arañazos y nanoscopios universales. El amplio rango dinámico de medidas de fuerza y ​​desplazamiento permite que los materiales, desde polímeros blandos hasta metales, se prueben con precisión y repetibilidad. Las opciones modulares se pueden adaptar a una variedad de aplicaciones: mapas de propiedades de materiales, pruebas de frecuencia, pruebas de rasguño y desgaste y pruebas de alta temperatura. INano ofrece una gama completa de opciones para expandir las pruebas, incluyendo calentamiento de muestras, medición continua de rigidez, mapeo de propiedades NanoBlitz3D / 4D y la opción de video remoto.

 

El iNano está equipado con el actuador InForce 50 para llevar a cabo nanoindentación universal y pruebas nanomecánicas. La alta resolución de carga  y alto rango de desplazamiento del InForce 50 permiten que el sistema realice una amplia gama de pruebas. El software InView es un paquete de software flexible y moderno que facilita las pruebas a nanoescala. El iNano es una plataforma compacta con un controlador InQuest de alta velocidad y un pórtico de aislamiento de vibraciones integrado en la carcasa. Se puede probar una amplia gama de materiales y dispositivos, incluidos metales, cerámicas, compuestos, películas delgadas, recubrimientos, polímeros, biomateriales y geles.

VENTAJAS

- Preciso, flexible y fácil de usar
- Amplia gama de pruebas nanomecánicas.
- películas delgadas y materiales blandos

  • Actuador InForce 50 para medición de desplazamiento capacitivo y actuación de fuerza electromagnética con puntas intercambiables
  • Sistema de calibración de punta único integrado en el software para una calibración de punta rápida y precisa
  • Controlador electrónico de alta velocidad InQuest con velocidad de adquisición de datos de 100 kHz y constante de tiempo de 20 µs
  • Sistema de movimiento XY con soporte de muestra magnético de fácil montaje
  • Microscopio integrado con zoom digital para una orientación precisa de la indentacion
  • ISO 14577 y métodos de prueba estándar
  • Paquete de software InView con RunTest, ReviewData, informes
  • InFocus, capacitación en línea de InView University y aplicación móvil InView
Inano box
Inanosupport1

Opciones

Csm
Sample heating
Nb3d
Nb4d
Thin film pack
Probe dma
Biomaterials method pack
Scratch and wear testing method pack
Databurst
Inview review
Vibration isolation
Iv option
Remotevideooption
Tips

Continuous stiffness measurement (CSM)

Continuous stiffness measurement is used to quantify the dynamic properties of the material, such as the rate of deformation and the effects induced by frequency. The CSM technique involves oscillation of the probe during indentation to measure properties as a function of depth, force, time or frequency. The option comes with a constant stress rate experience that measures hardness and modulus as a function of depth or load, the most common test method used in universities and industry. CSM is also used for other advanced measurement options, including the ProbeDMA ™ method for storage and loss module measurements and AccuFilm ™ measurements independent of the substrate. The CSM is integrated with the InQuest controller and InView software to provide ease of use and data quality.

Heating of samples to 300 ° C

The sample heating option at 300 ° C allows the sample to be placed in a chamber for uniform heating while undergoing simultaneous testing with the InForce 1000 or InForce 50 actuators. The option includes a high temperature control precision, filling with inert gas to reduce oxidation and cooling to eliminate waste heat. ProbeDMA, AccuFilm, NanoBlitz and CSM are all compatible with the sample heating option.

NanoBlitz 3D

NanoBlitz 3D uses the InForce 50 or InForce 1000 actuator and a Berkovich tip to generate 3D maps of nanomechanical properties for high E factor materials (> 3GPa). NanoBlitz performs up to 100,000 withdrawals (300x300 matrix) at <1 second per withdrawal and provides Young's modulus (E), hardness (H) and stiffness (S) values at a specified load for each withdrawal from the network . The large number of tests allows increased statistical precision. The histogram graphs show several phases or materials. The NanoBlitz 3D package includes visualization and data processing functionalities.

NanoBlitz 4D

NanoBlitz 4D uses the InForce 50 or InForce 1000 actuator and a Berkovich tip to generate 4D maps of the nanomechanical properties of low W / O and high E materials (> 3GPa). NanoBlitz performs up to 10,000 withdrawals (30x30 matrix) every 5 to 10 seconds and provides Young's modulus (E), hardness (H) and stiffness (S) values as a function of the depth of each withdrawal in the matrix. NanoBlitz 4D uses a constant strain rate method. The package includes visualization and data processing functionalities.

AccuFilm ™ Thin Film Method Pack

AccuFilm is an InView test method based on the Hay-Crawford model to measure the properties of materials independent of the substrate using continuous stiffness measurement (CSM). AccuFilm corrects the influence of the substrate on the film measurements for hard films on soft substrates, as well as for soft films on hard substrates.

Biomaterials Method Pack

The Biomaterials Method Pack offers the possibility of measuring the complex module of biomaterials with shear modules of the order of 1 kPa, and uses continuous stiffness measurement (CSM). The pack includes a flat tip and a test method to assess the viscoelastic properties. This measurement technique is essential for characterizing small-scale biomaterials that are not well served by traditional rheometric instruments.

Survey Scanning

The Biomaterials Method Pack offers the possibility of measuring the complex module of biomaterials with shear modules of the order of 1 kPa, and uses continuous stiffness measurement (CSM). The pack includes a flat tip and a test method to assess the viscoelastic properties. This measurement technique is essential for characterizing small-scale biomaterials that are not well served by traditional rheometric instruments.

Scratch and wear test method

The scratch test involves applying a constant or ramped load to an indenter while crossing the surface of the sample at a specified speed. Scratch tests make it possible to characterize many materials such as thin films, fragile ceramics and polymers.

DataBurst

DataBurst allows systems with InView software and the InQuest controller to record displacement data at speeds> 1 kHz for the measurement of strain loads, jumps and other high-speed events. IMicro systems with the user method development option can also modify the methods for working with DataBurst.

Development of user methods for InView control software

InView is a powerful and intuitive platform for experiential scripting that can be used to design new or complex experiments. Experienced users can configure and perform virtually any small-scale mechanical test using the iMicro system equipped with the exclusive InView option.

Active vibration isolation with the modular rack system
The optional high performance active vibration isolation system provides additional vibration isolation for the iMicro nanoindentator, in addition to its built-in vibration isolation. This easy-to-install system reduces vibration within six degrees of freedom, without any adjustments. A modular rack system contains all of the components in an integrated rack.

True Test I-V Electrical measurements

Controlled via InView software, the True Test I-V option for the iMicro nanoindentor uses a precision ammeter and a voltage source, an electrical path crossing the tip and a conductive tip. This design allows the user to apply specific voltages to a sample and measure the tip current while simultaneously actuating the InForce 50 or InForce 1000 actuator.

Remote video option

The remote video option provides two additional viewing angles in the iNano chamber, in addition to the existing microscope objective. A holder is mounted to focus on the tip of the indenter during the test, an ideal configuration for bending and soft materials. The second support is mounted on the gantry to visualize both the sample and the microscope objective during the configuration of the test. The switching of the view between the standard microscope objective and the USB camera is software controlled.

Indentation tips and calibration samples

The InForce 50, InForce 1000 and Gemini actuators use interchangeable tips. A wide variety of vivid penetrations are available, such as Berkovich, cube corner and Vickers, as well as flat punches, sphere punches and other geometries. Standard reference materials and calibration standards are also available for the entire product range.

Contáctenos para más información sobre este producto

¿Quieres una estimación?

¿Información Adicional?

Le responderemos dentro de las 24 horas.

 

  • Este campo está oculto cuando se visualiza el formulario


NAVEGACIÓN

- Productos de análisis de superficie

- Nuestros servicios

- Formación

- Servicio postventa

EMPRESA

- ScienTec Ibérica

- Contactos

- Noticias

SÍGUENOS

Newsletter

- Newsletter

- Facebook

- Linkedin

Logo-footer-sti

00 34 91 842 94 67

info@scientec.es

© 2019 Scientec Ibérica. All Rights Reserved.